XIANYUAlloy · Changzhou
Selection notes

Four comparisons that decide a specification

Each note takes two alloys, puts the numbers side by side, and says which one wins for which job — including when the answer is neither.

vs

Constantan vs Manganin

Both are copper-nickel-ish alloys with roughly half a micro-ohm-metre of resistivity. The decision is usually made by three numbers and one workshop reality.

vs

Nickel 200 vs Nickel 201

Same resistivity, same density, same drawing route. One number separates them, and it only matters above 315 °C.

vs

Type K vs Type E

Type E gives you nearly twice the signal. Type K gives you twice the range. Almost every other difference follows from those two facts.

vs

Manganin 6J12 vs 6J13

Two grades from the same family, differing mainly in resistivity level. The choice is usually made by the resistance value the design needs, not by a property table.

Send the specification — diameter, grade, temper, quantity.

We come back with a confirmed lead time and the documentation we can issue for the shipment. 100 g sample at cost; orders from 1 kg.

Request a quotation Order a 100 g sample